(a) The annealing of wrought iron gear required by this part shall be accomplished at a temperature between 1100° and 1200° F. and the exposure shall be of between 30 and 60 minutes duration. After being annealed, the gear shall be allowed to cool slowly and shall then be carefully inspected. All annealing shall be carried out in a closed furnace.
(b) When heat treatment of loose gear made of other than wrought iron or steel is recommended by the manufacturer, it shall be carried out in accordance with the specifications of the manufacturer.
Cite this article: FindLaw.com - Code of Federal Regulations Title 29. Labor § 29.1919.36 Heat treatment - last updated January 02, 2025 | https://codes.findlaw.com/cfr/title-29-labor/cfr-sect-29-1919-36/
FindLaw Codes may not reflect the most recent version of the law in your jurisdiction. Please verify the status of the code you are researching with the state legislature before relying on it for your legal needs.
A free source of state and federal court opinions, state laws, and the United States Code. For more information about the legal concepts addressed by these cases and statutes, visit FindLaw’s Learn About the Law.
Get help with your legal needs
FindLaw’s Learn About the Law features thousands of informational articles to help you understand your options. And if you’re ready to hire an attorney, find one in your area who can help.
Search our directory by legal issue
Enter information in one or both fields (Required)